FOR BUSINESS

Paving Grade Bitumen 50/70

Reference standard: EN 12591:2009

Description of the product

Paving grade bitumen 50/70 can be used primarily for asphalt concrete (AC) and stone mastic asphalt (SMA) in wearing courses, provided that the mixture complies with the requirements concerning resistance to rutting. The use of 50/70 bitumen for the production of base and binder courses also requires the verification of the mixture’s resistance to rutting. The use of 50/70 bitumen for the production of any layer of pavement designed to carry heavy, slow traffic (slow lanes, approaches to crossroads, etc.) is not recommended.​

Properties

Property Unit Test method Requrement
Penetration at 25°C
0.1 mm EN 1426 50 - 70
Softening point​ °C EN 1427 46 - 54
Resistance to hardening at 163°C   EN 12607-1 (RTFOT method) -
Retained penetration​ % EN 12607-1​ (RTFOT method) ≥ 50
Increase in Softening point ​°C EN 12607-1​ (RTFOT method) ≤ 9
Change of mass* (absolute value) ​% EN 12607-1​ (RTFOT method) ≤ 0.5
Flash point °C EN ISO 2592 ≥ 230​
Solubility % (m/m) EN 12592 ≥ 99.0

* Change of mass may be a positive or negative value